27/05/2016


From the anti electrostatic floor thickness, anti electrostatic floor standard thickness in the south is 0.8mm/1.0mm/1.2mm/1.5mm, while in the north, is more than 1.2mm. Poor quality anti-static floor is generally not up to this thickness, which will lead to the use of anti - static floor of the service life of the floor.

In anti - static flooring thickness, inferior antistatic floor will not up to the standard thickness, shoddy work, such as the thickness from 0.8mm down to 0.3mm, 0.4mm, so the thickness simply not up to the necessary strength, easy to cause anti electrostatic floor fracture. Beam tube wall thickness from 0.8mm/1.0mm thinned down to 0.3mm, 0.4mm for beam soft cause around the floor side tilt, caused serious floor collapse and fracture problems.